Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 4.14 MPa @Temperature 149 °C |
600 psi @Temperature 300 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% .. |
|||
Shear Strength | 4.14 MPa @Temperature 149 °C |
600 psi @Temperature 300 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Shear Strength | 4.14 MPa @Time 3600 sec |
600 psi @Time 1.00 hour |
Overlap, PVC |
3M Scotch-Weld™ EZ250030 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Shear Strength | 4.14 MPa @Temperature 149 °C |
600 psi @Temperature 300 °F |
Aluminum Overlap |
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive 3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°.. |