Shear Strength 52.0 MPa

@Temperature 232 °C
7540 psi

@Temperature 450 °F
Short Beam; Control (Prepreg with no freezer or out time exposure)
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel
Shear Strength 52.0 MPa

@Temperature 100 °C
7540 psi

@Temperature 212 °F
ILSS; prEN2563
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/48280/1000 Fabric
Fiber: T1000 12K 5H Satin, 283 g/m2Information provided by HexCel
Shear Strength 52.0 MPa

@Temperature 120 °C
7540 psi

@Temperature 248 °F
ILSS; prEN2563
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G1089/1000 Fabric
Fiber: T800H 6K 2x2 Twill, 200 g/m2Information provided by HexCel