Mechanical Properties Metric English Comments
Shear Strength 50.3 MPa

@Temperature 23.9 °C
7300 psi

@Temperature 75.0 °F
Short-Beam, Dry, Autoclave; ASTM D2344
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 3k 5HS Carbon Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Shear Strength 50.3 MPa

@Temperature 71.1 °C
7300 psi

@Temperature 160 °F
Short-Beam, Dry; Oven Cure 250°F, 90 min; ASTM D2344
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra..
Shear Strength 50.3 MPa

@Temperature 82.2 °C
7300 psi

@Temperature 180 °F
Short-Beam, Wet; Autoclave Cured; ASTM D2344
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, 6K 4HS IM7 Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 50.3 MPa

@Temperature 121 °C
7300 psi

@Temperature 250 °F
Short Beam, Wet
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber
Information provided by HexCel