Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 27.0 MPa @Temperature 232 °C |
3920 psi @Temperature 450 °F |
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64%; Wet condition-96 hours in boiling H2O |
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel |
|||
Shear Strength | 27.0 MPa @Temperature 80.0 °C |
3920 psi @Temperature 176 °F |
Lap Shear; Cured 5 days at 23°C; Substrate: 2024 T3 Aluminum Alloy (CSA pretreated, Unprimed); EN2243-1 |
Hexcel® Redux® 870 A/B Two Component Shimming and Potting Epoxy Paste Adhesive Redux 870 A/B is a two component high performance epoxy paste adhesive, ideal for use as a Liquid Shim or for potting applications. This high temperature performing thixotropic adhesive has been spe.. |