Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 26.5 MPa @Temperature 25.0 °C |
3840 psi @Temperature 77.0 °F |
Bond; Aluminum to aluminum, 1" overlap |
Lord Adhesives Circalokâ„¢ 6037 Epoxy Adhesive Circalokâ„¢ 6037 is an epoxy adhesive formulated for use by the semiconductor industry. An easy-to-spread thixotropic paste, it offers high heat transfer, low shrinkage, and a coefficient of ther.. |