Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 38.0 MPa @Temperature 21.1 °C |
5510 psi @Temperature 70.0 °F |
Lap Shear |
Hexcel® Redux® 312/5 Modified epoxy film adhesive Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Shear Strength | 38.0 MPa @Temperature 22.2 °C |
5510 psi @Temperature 72.0 °F |
Lap Shear, Primed with Redux 119 |
Hexcel® Redux® 319A High Performance Modified Epoxy Film Adhesive (0.08 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 38.0 MPa @Temperature 90.0 °C |
5510 psi @Temperature 194 °F |
0°, Interlaminar, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, AS4-C Fiber Designation: C193PW, Plain weaveInformation provided by HexCel |
|||
Shear Strength | 38.0 MPa @Temperature 20.0 °C |
5510 psi @Temperature 68.0 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |