Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 26.0 MPa @Temperature 149 °C |
3770 psi @Temperature 300 °F |
Lap Shear, Primed with Redux 119 |
Hexcel® Redux® 319 High Performance Modified Epoxy Film Adhesive (0.07 psf) Redux 319 is a high performance modified epoxy film adhesive curing at 350°F. It is available in both supported and unsupported versions at areal weights between 0.03 and 0.08 psf. The supported ve.. |
|||
Shear Strength | 26.0 MPa @Temperature 149 °C |
3770 psi @Temperature 300 °F |
Lap Shear |
Hexcel® Redux® 322U Modified epoxy film adhesive (0.06 psf) Redux 322 is a high performance modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures, where operating temperatures are experienced up .. |
|||
Shear Strength | 26.0 MPa @Temperature 132 °C |
3770 psi @Temperature 270 °F |
Short Beam |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |