Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 2.41 MPa @Temperature 24.0 °C |
350 psi @Temperature 75.2 °F |
Overlap, 1/8 birch to 1/8 birch, bond tested after aging 3 weeks @ 24°C and 50% RH at a separation rate of 0.2 in/min; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 2.41 MPa @Time 605000 sec |
350 psi @Time 168 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 25°C at 50% RH Aged; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 2.41 MPa @Time 605000 sec |
350 psi @Time 168 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 2.41 MPa @Time 1.21e+6 sec |
350 psi @Time 336 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 25°C at 50% RH Aged; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 2.41 MPa @Time 1.21e+6 sec |
350 psi @Time 336 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 2.41 MPa @Time 1.81e+6 sec |
350 psi @Time 504 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 25°C at 50% RH Aged; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Shear Strength | 2.41 MPa @Time 1.81e+6 sec |
350 psi @Time 504 hour |
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002 |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |