Shear Strength 2.41 MPa

@Temperature 24.0 °C
350 psi

@Temperature 75.2 °F
Overlap, 1/8 birch to 1/8 birch, bond tested after aging 3 weeks @ 24°C and 50% RH at a separation rate of 0.2 in/min; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 2.41 MPa

@Time 605000 sec
350 psi

@Time 168 hour
Overlap of Build-Up, 1/8 birch to 1/8 birch, 25°C at 50% RH Aged; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 2.41 MPa

@Time 605000 sec
350 psi

@Time 168 hour
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 2.41 MPa

@Time 1.21e+6 sec
350 psi

@Time 336 hour
Overlap of Build-Up, 1/8 birch to 1/8 birch, 25°C at 50% RH Aged; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 2.41 MPa

@Time 1.21e+6 sec
350 psi

@Time 336 hour
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 2.41 MPa

@Time 1.81e+6 sec
350 psi

@Time 504 hour
Overlap of Build-Up, 1/8 birch to 1/8 birch, 25°C at 50% RH Aged; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 2.41 MPa

@Time 1.81e+6 sec
350 psi

@Time 504 hour
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..