Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 3.03 MPa @Temperature 82.0 °C |
440 psi @Temperature 180 °F |
Overlap, Maple |
3M Scotch-Weld™ TE030 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 3.03 MPa @Temperature -40.0 °C |
440 psi @Temperature -40.0 °F |
Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 3.03 MPa @Temperature -40.0 °C |
440 psi @Temperature -40.0 °F |
Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ 3535 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Shear Strength | 3.03 MPa @Temperature -40.0 °C |
440 psi @Temperature -40.0 °F |
Overlap, ABS, Substrate Failure |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |