Mechanical Properties Metric English Comments
Shear Strength 15.1 MPa

@Temperature -55.0 °C
2190 psi

@Temperature -67.0 °F
Tube Shear; Dry; 20 min @ 175°C; EN2667-2
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic..