Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 15.1 MPa @Temperature -55.0 °C |
2190 psi @Temperature -67.0 °F |
Tube Shear; Dry; 20 min @ 175°C; EN2667-2 |
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic.. |