Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 12.1 MPa @Temperature 23.0 °C |
1760 psi @Temperature 73.4 °F |
Overlap, PVC, Substrate Failure |
3M Scotch-Weld™ TE030 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 12.1 MPa @Temperature 23.0 °C |
1760 psi @Temperature 73.4 °F |
Overlap, Polycarbonate |
3M Scotch-Weld™ TE015 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |