Polymer Property : Shear Strength = 1600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 11.0 MPa

@Temperature 150 °C
1600 psi

@Temperature 302 °F
Lap Shear; Cured 5 days at 23°C; Substrate: 2024 T3 Aluminum Alloy (CSA pretreated, Unprimed); EN2243-1
Hexcel® Redux® 870 A/B Two Component Shimming and Potting Epoxy Paste Adhesive
Redux 870 A/B is a two component high performance epoxy paste adhesive, ideal for use as a Liquid Shim or for potting applications. This high temperature performing thixotropic adhesive has been spe..
Shear Strength 11.0 MPa

@Temperature 177 °C
1600 psi

@Temperature 351 °F
Short Beam
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel
Shear Strength 11.0 MPa

@Temperature 93.3 °C
1600 psi

@Temperature 200 °F
Lap Shear
Hexcel® Redux® 335M Adhesive film for bonding metallic and composite components (0.03 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Shear Strength 11.0 MPa

@Temperature 80.0 °C
1600 psi

@Temperature 176 °F
Double Lap Shear; Dry; 60 min @ 120°C; Hexcel IS202
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic..