Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 15.0 MPa @Temperature 132 °C |
2180 psi @Temperature 270 °F |
Short Beam |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |