Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 12.8 MPa @Temperature 65.6 °C |
1850 psi @Temperature 150 °F |
ASTM D732 |
Greene Tweed Avalon® 56 PTFE PTFE is used in many pharmaceutical-sealing applications. Its chemical inertness and ultra-low level extractables provide pharmaceutical process and validation engineers with a safe material to use.. |