Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 77.9 MPa @Temperature 21.1 °C |
11300 psi @Temperature 70.0 °F |
Short-Beam, Dry; Autoclave Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 6K 5HS Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 77.9 MPa @Temperature 90.6 °C |
11300 psi @Temperature 195 °F |
0° Short Beam, Wet |
Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber Information provided by HexCel |
|||
Shear Strength | 78.0 MPa @Temperature 23.0 °C |
11300 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M55J Fiber Information provided by HexCel |