Polymer Property : Shear Strength = 10700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 73.8 MPa

@Temperature 82.2 °C
10700 psi

@Temperature 180 °F
Beam, V-Notched; Wet; Vacuum/Oven Cured; ASTM D5379-93
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 74.0 MPa

@Temperature 24.0 °C
10700 psi

@Temperature 75.2 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric
Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel