Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.5109 MPa @Shear Rate 5000 1/s, Temperature 260 °C |
74.10 psi @Shear Rate 5000 1/s, Temperature 500 °F |
ISO 11403-1 -2 |