Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.3325 MPa @Shear Rate 5000 1/s, Temperature 270 °C |
48.23 psi @Shear Rate 5000 1/s, Temperature 518 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers |