Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.2309 MPa @Shear Rate 500 1/s, Temperature 240 °C |
33.48 psi @Shear Rate 500 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |