Shear Strength 0.013929 MPa

@Shear Rate 10.0 1/s,
Temperature 240 °C
2.0202 psi

@Shear Rate 10.0 1/s,
Temperature 464 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers