Mechanical Properties Metric English Comments
Shear Strength 0.01013 MPa

@Shear Rate 10.0 1/s,
Temperature 280 °C
1.469 psi

@Shear Rate 10.0 1/s,
Temperature 536 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® 42A NC010 Nylon 66  (Unverified Data**)
Unreinforced High Viscosity Polyamide 66Zytel 42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers