Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 96.5 MPa @Thickness 1.57 mm |
14000 psi @Thickness 0.0620 in |
LW; ASTM D790 |
Industrial Laminates/Norplex NP101 Synthetic Fabric Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp.. |
|||
Flexural Strength | 96.5 MPa @Thickness 1.57 mm |
14000 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP615 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated .. |
|||
Flexural Strength | 96.5 MPa @Thickness 1.57 mm |
14000 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP318 Cotton Fabric Description: Post-forming canvas phenolic material. Mechanical and electrical properties similar to NP310E. It is made from a cotton fabric weighing more than 4 ounces per square yard and having a t.. |