Mechanical Properties Metric English Comments
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
CW
Industrial Laminates/Norplex ES-1 Engraving Stock
Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620”, 0.125”, and 0.500”
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex ES-1 Engraving Stock
Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620”, 0.125”, and 0.500”
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
CW
Industrial Laminates/Norplex ES-2 Engraving Stock
Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies.
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex ES-2 Engraving Stock
Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies.
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
CW
Industrial Laminates/Norplex ES-3 Engraving Stock
Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin.
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex ES-3 Engraving Stock
Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin.
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP320U Cotton Fabric
Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500"
Flexural Strength 93.1 MPa

@Thickness 1.57 mm
13500 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP310U Cotton Fabric
Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0...