Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 93.1 MPa @Thickness 1.57 mm |
13500 psi @Thickness 0.0620 in |
CW |
Industrial Laminates/Norplex ES-1 Engraving Stock Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620â€, 0.125â€, and 0.500†|
|||
Flexural Strength | 93.1 MPa @Thickness 1.57 mm |
13500 psi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex ES-1 Engraving Stock Description: Composed of white melamine paper core with various pigmented cover sheets.Thickness Tested: 0.0620â€, 0.125â€, and 0.500†|
|||
Flexural Strength | 93.1 MPa @Thickness 1.57 mm |
13500 psi @Thickness 0.0620 in |
CW |
Industrial Laminates/Norplex ES-2 Engraving Stock Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies. |
|||
Flexural Strength | 93.1 MPa @Thickness 1.57 mm |
13500 psi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex ES-2 Engraving Stock Description: Composed of black phenolic paper core, sub surfaces of white melamine, and various pigmented cover plies. |
|||
Flexural Strength | 93.1 MPa @Thickness 1.57 mm |
13500 psi @Thickness 0.0620 in |
CW |
Industrial Laminates/Norplex ES-3 Engraving Stock Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin. |
|||
Flexural Strength | 93.1 MPa @Thickness 1.57 mm |
13500 psi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex ES-3 Engraving Stock Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin. |
|||
Flexural Strength | 93.1 MPa @Thickness 1.57 mm |
13500 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP320U Cotton Fabric Description: Utility version of NP320E. Meets most, but not all, NEMA properties for L and LE, and is not certifiable as a NEMA Grade.Thickness Tested: 0.062", 0.125", and 0.500" |
|||
Flexural Strength | 93.1 MPa @Thickness 1.57 mm |
13500 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP310U Cotton Fabric Description: Utility grade canvas phenolic with properties similar to NP310E.Not certifiable to NEMA due to low crosswise flexural strength. Previously designated NP310C.Thickness Tested: 0.062", 0... |
|||
Flexural Strength | 93.0 MPa @Temperature 23.0 °C |
13500 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 2.7%); ASTM-D790 |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |