Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 6.00 MPa @Temperature 80.0 °C |
870 psi @Temperature 176 °F |
Practical Use (Water Absorption 2.0%); ASTM-D790 |
Toyobo GLAMIDE® T-222SA Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |