Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 490 MPa @Treatment Temp. 50.0 °C, Time 3600 sec |
71100 psi @Treatment Temp. 122 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |