Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 490 MPa @Temperature 71.1 °C |
71000 psi @Temperature 160 °F |
Wet; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 3K PW Carbon Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Strength | 490 MPa @Temperature 23.9 °C |
71000 psi @Temperature 75.0 °F |
Dry; 325°F Autoclave Cured; ASTM D790 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 7781 E-Glass Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Flexural Strength | 490 MPa @Treatment Temp. 50.0 °C, Time 3600 sec |
71100 psi @Treatment Temp. 122 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |