Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 49.0 MPa @Temperature 23.0 °C |
7110 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 3.5%); ASTM-D790 |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 49.0 MPa @Temperature 150 °C |
7110 psi @Temperature 302 °F |
ASTM D790 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |