Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 475 MPa @Temperature 23.0 °C |
68900 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica.. |
|||
Flexural Strength | 475 MPa @Thickness >=1.60 mm, Temperature 100 °C |
68900 psi @Thickness >=0.0630 in, Temperature 212 °F |
Perpendicular to laminations; EN 60893 |
HOS-Technik Homide 250 Bismaleimide Resin Homide 250 is a prepolymer bismaleimide resin system with a low softening range of 90-125°C supplied in powder form. The resin can be cured thermally to create a cross-linked thermoset with excel.. |