Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 65300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 450 MPa

@Thickness >=1.50 mm
65300 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Flexural Strength 450 MPa

@Treatment Temp. 20.0 °C,
Time 3600 sec
65300 psi

@Treatment Temp. 68.0 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets
Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t..
Flexural Strength 450 MPa

@Thickness >=1.50 mm
65300 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V..
Flexural Strength 450 MPa

@Thickness >=1.50 mm
65300 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets
Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation ..
Flexural Strength 450 MPa

@Thickness >=1.50 mm
65300 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Flexural Strength 450 MPa

@Thickness >=1.50 mm
65300 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c..
Copyright © lookpolymers.com All Rights Reserved