Mechanical Properties Metric English Comments
Flexural Strength 417 MPa

@Thickness 1.57 mm
60500 psi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex NP185 Carbon Fiber  (discontinued **)
Description: NP185, aramid fiber fabric/phenolic surfaces (2 ply each side) on NP504 core material. Excellent mechanical properties at elevated temperatures and in adverse environments. Used as wear..