Industrial Laminates/Norplex NP185 Carbon Fiber  (discontinued **)

Category Polymer , Thermoset , Aramid , Carbon Fiber/Thermoset Composite , Phenolic
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industrial Laminates/Norplex NP185 Carbon Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NP185, aramid fiber fabric/phenolic surfaces (2 ply each side) on NP504 core material. Excellent mechanical properties at elevated temperatures and in adverse environments. Used as wear strips in high temperature environments.Thickness Tested: 0.250"
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
Moisture Absorption at Equilibrium 1.32 %

@Thickness 1.57 mm
1.32 %

@Thickness 0.0620 in
Mechanical Properties Metric English Comments
Flexural Strength 303 MPa

@Thickness 1.57 mm
43900 psi

@Thickness 0.0620 in
CW
417 MPa

@Thickness 1.57 mm
60500 psi

@Thickness 0.0620 in
LW
Izod Impact, Unnotched 5.55 J/cm

@Thickness 12.7 mm
10.4 ft-lb/in

@Thickness 0.500 in
CW, E-48/50
6.30 J/cm

@Thickness 12.7 mm
11.8 ft-lb/in

@Thickness 0.500 in
LW, E-48/50
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 170 °C
338 °F
Maximum Operating Temperature
Users viewing this material also viewed the following: