Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 345 MPa @Temperature 216 °C |
50000 psi @Temperature 420 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Flexural Strength | 345 MPa @Temperature 23.9 °C |
50000 psi @Temperature 75.0 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Flexural Strength | 345 MPa @Temperature 177 °C |
50000 psi @Temperature 350 °F |
Dry, Autoclave with Post-Cure; ASTM D790 |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Flexural Strength | 345 MPa @Temperature 23.9 °C |
50000 psi @Temperature 75.0 °F |
Dry; Post-Cure; ASTM D790 |
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low .. |
|||
Flexural Strength | 345 MPa @Thickness 1.57 mm |
50000 psi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex NP841 Glass Fabric
(discontinued **) Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: .. |
|||
Flexural Strength | 345 MPa @Temperature 23.0 °C |
50000 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-663G50A MXD66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 345 MPa @Temperature -40.0 °C |
50000 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 345 MPa @Temperature 150 °C |
50000 psi @Temperature 302 °F |
ISO 178 |
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex.. |