Mechanical Properties Metric English Comments
Flexural Strength 345 MPa

@Temperature 216 °C
50000 psi

@Temperature 420 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Flexural Strength 345 MPa

@Temperature 23.9 °C
50000 psi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f..
Flexural Strength 345 MPa

@Temperature 177 °C
50000 psi

@Temperature 350 °F
Dry, Autoclave with Post-Cure; ASTM D790
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Flexural Strength 345 MPa

@Temperature 23.9 °C
50000 psi

@Temperature 75.0 °F
Dry; Post-Cure; ASTM D790
Park Electrochemical Nelcote® V-341 Polybutadiene Prepreg, 503 Quartz Reinforced
Nelcote® V-341 is Polybutadiene resin system designed to provide excellent electrical properties in demanding airborne, shipboard, and undersea applications.Key Features and Benefits:Extremely low ..
Flexural Strength 345 MPa

@Thickness 1.57 mm
50000 psi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex NP841 Glass Fabric  (discontinued **)
Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: ..
Flexural Strength 345 MPa

@Temperature 23.0 °C
50000 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 345 MPa

@Temperature -40.0 °C
50000 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 345 MPa

@Temperature 150 °C
50000 psi

@Temperature 302 °F
ISO 178
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex..