Polymer Property : Flexural Strength = 34100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 235 MPa

@Strain 5.00 %
34100 psi

@Strain 5.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS.
Flexural Strength 235 MPa

@Temperature -40.0 °C
34100 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-402FR Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..