Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 235 MPa @Strain 5.00 % |
34100 psi @Strain 5.00 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Flexural Strength | 235 MPa @Temperature -40.0 °C |
34100 psi @Temperature -40.0 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-402FR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |