Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 310 MPa @Strain 4.00 % |
45000 psi @Strain 4.00 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 310 MPa @Temperature -40.0 °C |
45000 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 1.25%); ASTM-D790 |
Toyobo GLAMIDE® T-663G50 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 310 MPa @Temperature 23.0 °C |
45000 psi @Temperature 73.4 °F |
Practical Use (Water Absorption 0.8%); ASTM-D790 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |