Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 26800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 185 MPa

@Temperature 175 °C
26800 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK -HT™ 22CA30 PolyEtherKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact com..
Flexural Strength 185 MPa

@Strain 6.00 %
26800 psi

@Strain 6.00 %
Conditioned; ISO 178
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
Flexural Strength 185 MPa

@Strain 5.00 %
26800 psi

@Strain 5.00 %
ISO 178
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres
PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp
Flexural Strength 185 MPa

@Strain 5.00 %
26800 psi

@Strain 5.00 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS.
Flexural Strength 185 MPa

@Temperature 80.0 °C
26800 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-663G30 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 185 MPa

@Temperature -40.0 °C
26800 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 185 MPa

@Temperature 23.0 °C
26800 psi

@Temperature 73.4 °F
Result based on HT G22; ISO 178
Victrex® HT™ G45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia..
Copyright © lookpolymers.com All Rights Reserved