Mechanical Properties Metric English Comments
Flexural Strength 179 MPa

@Thickness 1.57 mm
26000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP329 Cotton Fabric
Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, ..
Flexural Strength 179 MPa

@Thickness 8.00 mm
26000 psi

@Thickness 0.315 in
CW
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric
Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined..
Flexural Strength 179 MPa

@Thickness 1.57 mm
26000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..
Flexural Strength 179 MPa

@Temperature -40.0 °C
26000 psi

@Temperature -40.0 °F
ASTM D790
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..