Polymer Property : Flexural Strength = 165 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
Flexural Strength 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
50%RH; ISO 178
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSL NC010 is a 25% glass fiber reinforced, heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Flexural Strength 165 MPa

@Thickness 1.57 mm
24000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..
Flexural Strength 165 MPa

@Temperature -40.0 °C
23900 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.3%); ASTM-D790
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 381G Medium Viscosity
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD..
Flexural Strength 165 MPa

@Temperature 23.0 °C
23900 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..