Mechanical Properties Metric English Comments
Flexural Strength 89.6 MPa

@Temperature 232 °C
13000 psi

@Temperature 450 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only..
Flexural Strength 89.6 MPa

@Thickness 1.57 mm
13000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP193M Synthetic Fabric Base Grade
Description: 17 oz. aramide and “soft glass” fibers are combined to make a fabric that is stronger than pure aramide and less abrasive than glass fabrics. This material is impregnated with..
Flexural Strength 89.6 MPa

@Thickness 1.57 mm
13000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP691 Paper Base Laminate
Description: Flame resistant, room temperature punching grade. NP691 is very similar to NP612 in electrical properties and mechanical strength, with improved moisture resistance.Thickness Tested: 0...
Flexural Strength 89.6 MPa

@Temperature 232 °C
13000 psi

@Temperature 450 °F
ASTM D790
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not ..
Flexural Strength 89.6 MPa

@Temperature 23.9 °C
13000 psi

@Temperature 75.0 °F
ASTM D790
Saint-Gobain Meldin® 7022 CM Compression Molded Graphite Filled Polyimide
Melidin® 7022 CM is a compression molded polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin..