Mechanical Properties Metric English Comments
Flexural Strength 75.9 MPa

@Temperature 23.0 °C
11000 psi

@Temperature 73.4 °F
ASTM D790
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L
Flexural Strength 75.8 MPa

@Thickness 1.57 mm
11000 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP101 Synthetic Fabric
Description: Phenolic resin combined with spun nylon fabric. Good impact strength and excellent electrical properties under high humidity conditions. Meets applicable Boeing specification, but exemp..
Flexural Strength 75.8 MPa

@Temperature 175 °C
11000 psi

@Temperature 347 °F
4; ISO 178
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Flexural Strength 75.8 MPa

@Temperature 23.9 °C
11000 psi

@Temperature 75.0 °F
ASTM D790
Saint-Gobain Meldin® 7211 DF Direct Formed Graphite and PTFE Filled Polyimide
Melidin® 7211 DF is a direct formed polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Specific..