Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Unnotched | 11.0 J @Thickness 1.00 - 6.00 mm |
8.10 ft-lb @Thickness 0.0394 - 0.236 in |
ASTM D256 |
CPC - Vycom CELTEC® Expanded Rigid foam PVC board Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface.. |