Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 156 kN/m | 890 pli | ASTM D624 (Die C) |
Lubrizol Advanced Materials PEARLTHANE® D11H92S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H92S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Tear Strength | 156 kN/m | 890 pli | ASTM D624 |
C.O.I.M. LARIPUR® LPR6260 PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |