Polymer Property : Tear Strength = 697 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 122 kN/m
697 pli
Die C; ISO 34-1B
Lubrizol Advanced Materials Pearlthane® ECO D12T90 Thermoplastic Polyurethane
Type : Pearlthane® ECO D12T90 is a high performance bio-based thermoplastic polyurethane. With ca. 38% bio-based content.Main Application : Injection MouldingSpecial Features : Very good flexibil..