Polymer Property : Tear Strength = 67.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 67.0 kN/m
382 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 67.0 kN/m
382 pli
ASTM D1938
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera..
Tear Strength 67.0 kN/m
382 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 67.0 kN/m
382 pli
ASTM D1938
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera..
Tear Strength 67.0 kN/m
382 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 67.0 kN/m
382 pli
ASTM D1938
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera..
Tear Strength 67.0 kN/m
382 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 67.0 kN/m
382 pli
ASTM D1938
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera..
Tear Strength 67.0 kN/m
382 pli
ASTM D1938
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera..
Tear Strength 67.0 kN/m
382 pli
ASTM D1938
A. Schulman INVISION™ FX-9090UE Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ FX-9090UE is a polyolefin-based thermoplastic of 90 Shore A durometer, which has been formulated soft touch, excellent scratch/mar resistance, low gloss, and excellent weathera..
Tear Strength 67.0 kN/m
382 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Tear Strength 67.0 kN/m
382 pli
with incision; ISO 34B
Lubrizol ESTANE® GP85AE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 85AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
Tear Strength 67.0 kN/m
382 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 67.0 kN/m
382 pli
ASTM D624
ELASTO UK Dryflex® 420351S SBS Based Material, 35D Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
Tear Strength 67.0 kN/m
382 pli
ASTM D624
ELASTO UK Dryflex® 422351S SBS Based Material, 35D Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
Tear Strength 67.0 kN/m
382 pli
Graves
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N774 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tear Strength 67.0 kN/m
382 pli
2 in/min; ASTM D624
A. Schulman POLYPUR™ FPU 1107 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.