Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 62.0 kN/m | 354 pli | ASTM D624 |
UBE UBEPOL VCR617 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tear Strength | 62.0 kN/m | 354 pli | ISO 34-B |
AlphaGary Evoprene™ G 964 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |