Polymer Property : Tear Strength = 6.60 kN/m
Polymer Property :
Tear Strength =
6.60 kN/m
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tear Strength
6.60
kN/m
37.7
pli
ASTM D624
Vicone High Performance Rubber VicoSilâ„¢ 159DLK-RD High Performance Silicone Rubber
Meets AMS 3302 Silicone 50 Durometer.